Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
This is the free Material Data Center Datasheet of RADILON ADLINE CS CF10 HP BK - PA666-CF - RadiciGroup High Performance Polymers
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces
Check here, which other Radilon A datasheets, application examples or technical articles are available in Material Data Center
Suitable for parts requiring stiffness, high dimensional stability and very reduced shrinkage. The material offers good surface aspect and easy processability.
机械性能 | 干 / 已调节 | 单位 | Test Standard | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
ISO数据 | |||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
拉伸模量 | 3850 / - | MPa | ISO 527 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
屈服应力 | 65 / - | MPa | ISO 527 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
屈服伸长率 | 3.5 / - | % | ISO 527 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
名义断裂伸长率 | 18 / - | % | ISO 527 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
无缺口简支梁冲击强度, +23°C | 60 / - | kJ/m² | ISO 179/1eU |
热性能 | 干 / 已调节 | 单位 | Test Standard | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
ISO数据 | |||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
熔融温度, 10°C/min | 195 / * | °C | ISO 11357-1/-3 |
其它性能 | 干 / 已调节 | 单位 | Test Standard |
吸水性 | 9 / * | % | 类似ISO 62 |
吸湿性 | 2.6 / * | % | 类似ISO 62 |
密度 | 1160 / - | kg/m³ | ISO 1183 |
In the case of granules, the material is delivered in moisture-proof packaging ready for processing. Maximum recommended water content for best processing is 0.10%. Typical conditions with a desiccant drier: temperature 80 ° C, dew point -20 ° C or below, time 2-4 h or more. In the case of filaments, the material is originally sealed in vacuum bags with silica gel inside to keep environment in dry conditions. For best printing results, it is recommended to pre-dry the filament at 70-80°C for 2-4 h or more. Alternatively, Radilon® Adline filaments are compatible with Drywise system from Thought3D Ltd.
Recommended 3D-Print processing parameters:
Nozzle Temperature | Bed Temperature | Adhesion promoter | Print Speed |
250°-280°C | 70-100°C | Magigoo glue | 30-40 mm/s |
Please note: Parameters are dependent on printer used.
Radici tests were performed on a Ultimaker S5 printer